| Application | Automotive Products, Braiding Hoses, Brushes, Chains, Conveyor Belts, Filters, Free Cutting Wires, Fasteners, Nails, Flexible Connectors, Kitchen Ware, and Gadgets |
| Diameter |
0.43 mm to 1.25 mm |
| Grades |
304 and 316 |
| Finish | Bright, Matte Finish, Soap Coated or Electro Polish Quality |
| Condition | Soft and Solution Annealed |
| Application | Commonly used in construction for binding materials, fencing, and reinforcing structures |
| Diameter |
0.30 mm to 1.2 mm |
| Standards |
IS: 280- 2006; IS: 398 |
| Zinc Coating | 20 to 60 Gsm/ SqMtr |
| Material |
Mild Steel / Stainless Steel |
| Thread Type |
Full Thread |
| Size | 8 * 13 |
| Head Type | Pan headed with neoprene washer |
| Application | Strapping on tanks and vessels |
| Material |
Stainless Steel / Aluminum |
| Seal Thickness |
0.5 mm to 0.8 mm |
| Strap Size | 12 mm to 25 mm |
| Strap Width | 13mm, 15mm, 20mm, 25mm, 40mm, 50mm |
| Packaging Type |
COIL |
| Material Grade |
Stainless Steel: 304 Aluminum: 408000, H14 |
| Thickness | 0.4mm up to 1.2mm |
| Strap Width | 13mm, 15mm, 20mm, 25mm, 40mm, 50mm |
| Color | Aluminum As confirmed by TSTM-01 |
| Composition | 0.012 mm Polyester Film 0.025 mm Aluminum Foil 0.012 mm Polyester Film |
| Weight | 160 ± 3 % g/m2 |
| Thickness | 50 ± 5% ㎛ (polyester film + Al foil) |
| Water vapour permeance | Below 0.005 perms (g/㎡ 24hr) |
| Service temperature | Temperature at the coated surface) - 70 ℃ ~ 150 ℃ As confirmed by TSTM-04 |
| Melting point | 250 ℃ (polyester) |
| Color | White As confirmed by TSTM-01 |
| Composition | Glass cloth fabric, leno weave with resin finish |
| Weight | Raw - 58 ± 5 g/㎡ Resin - ≥ 16 g/㎡ (resin content - ≥ 18 %) |
| Warp | 34×2 (tex) / 10 (counts/inch) |
| Color | Black As confirmed by TSTM-01 |
| Application | Trowel As confirmed by TSTM-06 |
| Density | 1.65± 0.05 ㎏/ℓ As confirmed by ASTM D 1475 |
| Coverage | 35.36 ㎏/㎡ (21.43 ℓ/㎡) Dried film thickness: 15 mm As confirmed by TSTM-07 |
| Service temperature limits | (Temperature at coated surface) - 100 ℃~ 600 ℃ (-148 ℉ ~ 1112 ℉) As confirmed by TSTM-04 |
| Heat transfer coefficient | 100 ~ 200 Kcal/㎡·hr·℃ 20.48 ~ 40.96 Btu/ft2 ·hr·℉ As confirmed by ASTM C 518 |
| Thermal conductivity | 10 ~ 12 Kcal/m·hr·℃ at 200 ℃ As confirmed by ASTM C 518 |
| Color | Aluminum (gray) As confirmed by TSTM-01 |
| Application | Caulking gun As confirmed by TSTM-06 |
| Density | 1.09 ± 0.05 ㎏/ℓ As confirmed by ASTM D 147 |
| Coverage | Caulking gun (330㎖ tube): - 38m @3.2mm bead As confirmed by TSTM-07 |
| Drying time | Set to touch: 30~60 minutes Dry through: 72 hours As confirmed by ASTM D 1640 |
| Service temperature limits | (Temperature at coated surface) - 101℃ ~ 141℃ (-150℉ ~ 28 As confirmed by TSTM-04 |
| Water Vapor permeance | ≤ 0.005 perms (DFT 1.3 mm) As confirmed by ASTM E 96 |
| Color | Beige (Off-White) As confirmed by TSTM-01 |
| Application | Trowel As confirmed by TSTM-06 |
| Density | 1.53 ± 0.05 ㎏/ℓ As confirmed by ASTM D 1475 |
| Coverage | 2.91 ㎏/㎡ (1.90 ℓ/㎡) Dried film thickness: 1.6 mm As confirmed by TSTM-07 |
| Drying time | Set to touch: 2 ~ 3 hours. Essentially non-drying As confirmed by ASTM D 1640 |
| Service temperature limits | (Temperature at coated surface) - 196 ℃ ~ 93 ℃ (-321 ℉ ~ 200 ℉) As confirmed by TSTM-04 |
| Water Vapor permeance | ≤ 0.02 perms (DFT 1.3 mm) As confirmed by ASTM E 96 |
| Color | TIC 4055 White / TIC 4056 Gray As confirmed by TSTM-01 |
| Application | Trowel or rubber glove As confirmed by TSTM-06 |
| Density | 1.20± 0.05 ㎏/ℓ As confirmed by ASTM D 1475 |
| Coverage | 3.43 ~ 5.14 ㎏/㎡ (2.86 ~ 4.28 ℓ/㎡) Dried film thickness: 1.2 ~ 1.8 mm As confirmed by TSTM-07 |
| Drying time | Set to touch: 5 hours Dry through: 48 hours As confirmed by ASTM D 1640 |
| Service temperature limits | (Temperature at coated surface) -46℃ ~ 121℃ (-51℉ ~ 250℉ As confirmed by TSTM-04 |
| Water Vapor permeance | ≤ 0.02 perms (DFT 1.3 mm) |
| Color | Beige As confirmed by TSTM-01 |
| Application | Trowel As confirmed by TSTM-06 |
| Density | 1.47 ± 0.05 ㎏/ℓ As confirmed by ASTM D 1475 |
| Coverage | 2.37 ㎏/㎡ (1.61 ℓ/㎡) Dried film thickness: 1.0 mm As confirmed by TSTM-07 |
| Bonding time range | 10 ~ 20 minutes As confirmed by TSTM-17 |
| Service temperature limits | (Temperature at coated surface) -59 ℃ ~ 150 ℃ (-74℉ ~ 302℉) As confirmed by TSTM-04 |
| Typical material | Foster 95-50 As per TIC 7020 |
| Typical material | Foster 81-33 TIC 5080 (one component) As per ASTM C871 |
| Foil composition: | 12 µm polyester film 25 µm aluminum foil 12 µm polyester film |
| Tensile strength | 100 MPa |
| Yield strength | 70 N / cm |
| Tear resistance | 400 g / mm |
| Temperature range | +120°C to -60°C |
| Water vapour permeability in acc. with ASTM E 96, procedure E (37.8°C, 90% RH) | Max. 10.10-6 g / (m².h.mmHg) |